Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced T1000HG6 LS BK - PA6T/6I-GF30 - BASF

Material Data Center offers the following functions for Ultramid® Advanced T1000HG6 LS BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Heat stabilized, partially aromatic polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures and excellent chemical resistance for highly stressed parts. Ultramid® Advanced T1000HG6 LS BK can be characterized as compound with high strength and stiffness, very low water absorption and outstanding dimensional stability. It features a high melting point (320°C) and excellent melt stability.

Markets & applications
Automotive: Fuel system, cooling system, powertrain, Auto E&E, sensors, pumps, fuel cell
Industry goods: Pumps, compressors
Consumer goods: Home appliances, consumer electronics
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Molding shrinkage, parallel 0.4 / * % ISO 294-4, 2577
Molding shrinkage, normal 1.0 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 11800 / 12000 MPa ISO 527
Stress at break 190 / 180 MPa ISO 527
Strain at break 1.9 / 1.7 % ISO 527
Charpy impact strength, +23°C 55 / 50 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 50 / 50 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 7.5 / 6.5 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 7 / 6.5 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 320 / * °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 130 / * °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 275 / * °C ISO 75-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Surface resistivity * / >1E15 Ohm IEC 62631-3-2
Electric strength 39 / - kV/mm IEC 60243-1
Comparative tracking index - / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 4.1 / * % Sim. to ISO 62
Humidity absorption 1.8 / * % Sim. to ISO 62
Density 1440 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 105 / * cm³/g ISO 307, 1157, 1628
Diagrams
Dynamic Shear modulus-temperature , Ultramid® Advanced T1000HG6 LS BK (dry), PA6T/6I-GF30, BASF
Dynamic Shear modulus-temperature , Ultramid® Advanced T1000HG6 LS BK (cond.), PA6T/6I-GF30, BASF
Stress-strain , Ultramid® Advanced T1000HG6 LS BK (dry), PA6T/6I-GF30, BASF
Stress-strain , Ultramid® Advanced T1000HG6 LS BK (cond.), PA6T/6I-GF30, BASF
Secant modulus-strain , Ultramid® Advanced T1000HG6 LS BK (dry), PA6T/6I-GF30, BASF
Secant modulus-strain , Ultramid® Advanced T1000HG6 LS BK (cond.), PA6T/6I-GF30, BASF
Tensile modulus-temperature , Ultramid® Advanced T1000HG6 LS BK (dry), PA6T/6I-GF30, BASF
Tensile modulus-temperature , Ultramid® Advanced T1000HG6 LS BK (cond.), PA6T/6I-GF30, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Special Characteristics
Heat stabilized or stable to heat
Features
Melt Strength
Chemical Resistance
General Chemical Resistance
Applications
Automotive, Electrical and Electronical
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 335 - 355 °C
injection molding, Melt temperature, recommended: 350 °C
injection molding, Mold temperature, range: 140 - 170 °C
injection molding, Mold temperature, recommended: 150 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.